Vanadium Oxide (VOx ) exists in various phases, its stoichiometry can be controlled so that it exhibits high Temperature Co-efficient of Resistance (TCR). This property makes it useful for bolometers used in infrared detectors/thermal cameras.
It may be deposited using Ion Beam Deposition (IBD).
Process results are highly repeatable with excellent uniformity of thickness and TCR.